PU Seal Casting Machine: Setting Shot Range and Tooling Banner background

PU Seal Casting Machine: Setting Shot Range and Tooling

A PU seal casting machine is sized by the shot, not by the largest number on the specification sheet. Seals are small, often thin-walled, and usually ...

A PU seal casting machine is sized by the shot, not by the largest number on the specification sheet. Seals are small, often thin-walled, and usually run in multi-cavity molds, so the figure that decides whether a 1A1B unit suits the job is the grams you must place in each cavity inside the material’s pot life, together with how tightly the head holds mix ratio at that shot size. Shot range and tooling are one decision: the mold defines the shot, the shot defines the machine, and the machine’s metering behaviour at that shot decides how much of the tooling investment you recover.

Why the seal geometry decides the machine size

A seal is a small part with an unforgiving requirement. The lip has to hold pressure, the body has to resist oil and compression set, and every dimension has to repeat across a long production run. Those requirements reach the machine as three inputs: the material volume each cavity takes, the flow path the mixed material must travel before the mold is full, and the time the formulation allows before viscosity rises past the point where the mold still fills.

Seal cross sections are thin compared with their length. A thin section gels quickly against the mold wall, so the fill has to finish before the leading edge of the material stops moving. That pushes toward a faster pour. Faster pouring, however, entrains air at gates and sharp corners, and it can jet across a cavity instead of filling from the bottom. The usable pour rate is a window rather than a maximum.

Multi-cavity tooling multiplies the shot without changing the per-cavity flow problem. Eight small cavities ask for eight times the material of one, delivered in roughly the same time, so the head and pumps run at a higher rate while each cavity still needs a controlled fill.

This is why headline output tells you very little on its own. What matters is whether the unit holds mix ratio and shot weight inside the band your mold actually uses. A seal shop running 15 to 90 g shots spends its whole working life at the low end of a casting machine’s range, where metering resolution, valve response and temperature stability matter more than the maximum flow printed in the brochure.

How shot weight defines the working range

Start with arithmetic, not with a machine. The material per mold is:

Shot weight per mold = cavity volume × cured density × cavity count × (1 + runner and overflow allowance)

Cavity volume comes from the mold drawing, not from the finished part envelope, because the cavity includes the overflow lip and any locating features. Cured density comes from your material supplier’s data for the specific formulation, measured on a cured sample rather than taken from the liquid component. The allowance covers sprue, runner and overflow, and on small seals it can be a larger share of the shot than buyers expect, because a thin cavity needs somewhere for the displaced air and the first, cooler material to go.

Take a four-cavity mold where each cavity holds 18 cm³ and the cured density is 1.1 g/cm³. Each cavity takes about 19.8 g, the mold takes about 79 g, and a 10 percent runner allowance brings the shot to roughly 87 g. Poured at 80 to 90 g/s, the fill lasts about one second.

Now take eight cavities of 1.5 cm³ at the same density. Each cavity holds about 1.65 g, so the whole shot is about 13 g. That mold sits below the controllable band of a unit rated from 20 g/s, and the fill would be over before the metering system settled into steady flow. The answer is not to add cavities until the number looks respectable. Either the machine is specified with a head sized for small shots, or the trial has to prove repeatability at the bottom edge before the tool is cut. A 20 to 500 g/s band is a wide envelope; most seal work happens in the first fifth of it.

Shot weight per mold, not the headline pour rate, is the number the rest of the specification hangs on. <How To Calculate Shot Weight In Polyurethane> covers the cavity volume and density calculation in more detail.

Where ratio and metering accuracy actually matter

Ratio error in a cast PU seal rarely appears as a visible fault on the day it happens. It appears later as a hardness band that drifts across cavities, a compression set result that fails after ageing, or a lip that swells more than expected in oil. That is why the ratio window on a seal casting machine is a process control statement, not a mixing convenience.

The two common chain extenders behave differently enough to change how the machine is configured. Published ranges for a 1A1B seal unit put MOCA at roughly 100:8 to 100:13 and BDO at roughly 100:3 to 100:6 against the prepolymer. Those windows are not interchangeable settings. MOCA is solid at room temperature and has to be held molten in a heated tank and line, which is why component B control runs around 90 to 115 °C on the MOCA route. BDO stays liquid and is controlled far lower, in the 25 to 50 °C region. Getting the wrong band means either solidified hardener in the line or an aged, discoloured component that changes the cure.

ItemMOCA routeBDO routeWhat it changes in the cell
Mix ratio window against prepolymerabout 100:8 to 100:13about 100:3 to 100:6Which formulations the machine can run without re-plumbing
Component B temperatureroughly 90 to 115 °Croughly 25 to 50 °CTank, line and head heating scope, plus heat-up time at start of shift
Handling at restSolid, must stay moltenLiquid at room temperatureShutdown, weekend and cleaning procedure
Typical property emphasisWear and compression resistanceResilience and reboundWhich seal duties the cell is aimed at
Changeover between the twoRequires full heat and purge cycleFaster, lower thermal massWhether one machine can serve mixed product families

Metering accuracy is the other number that gets misread. A dynamic accuracy of ±0.3 percent across the full range describes how the pumps and valves behave when they are working across the scale. At a 13 g shot the absolute error budget is set by valve response and by how long the machine spends in steady flow, not by the percentage alone. Ask for the accuracy basis, then verify it at your shot size during the trial.

Mixing quality follows the same logic. A head running at 8000 to 12000 rpm needs enough residence time and enough back pressure to blend two components of very different viscosity. Very small shots pass through the mixing chamber quickly, so the first material out of the head is the least mixed. That is one reason a purge shot before the mold closes is standard practice rather than waste.

Ratio error usually shows up first as a hardness and compression set shift, not as a visible defect. <Shore A Vs Shore D Hardness In Polyurethane> covers which scale applies to elastomer parts and how the two scales differ.

What the tooling has to do with the shot

Tooling quoted without cavity and runner volumes cannot be checked against a shot range, and that single omission causes more specification arguments than any machine parameter. Ask the moldmaker for four numbers before the machine is chosen: cavity volume, runner and overflow volume, cavity count, and the intended fill time.

Cavity layout then follows from the machine interface. A mold with cavities arranged far apart needs longer runners, which adds material to the shot and adds a cooler path for the leading edge. A compact layout shortens the runner but can crowd the venting. Vents belong at the last point to fill, and on a thin seal section that point moves when you change the pour rate, so vent location and pour rate have to be agreed together.

Mold material follows run length and tolerance rather than preference. Aluminium heats and cools quickly, which shortens cycles on prototypes and low-volume families, and it wears faster on abrasive filled systems. Steel holds cavity detail and withstands higher clamp and longer runs, at the cost of slower thermal response. For seal lips, the surface finish of the cavity face is part of the product specification, since a tool mark on the sealing face becomes a leak path.

Temperature control deserves the same attention as the shot. A mold running cold raises viscosity at the wall, which fights the fill and can produce cold laps at the lip. A mold running hot shortens pot life inside the cavity and can cause shrinkage at the thickest section after demold. The control channels, the number of circuits and the temperature unit capacity all belong in the tooling quotation, because retrofitting them later usually means a new mold half.

A practical check before signing: confirm the intended mold temperature, the demold time and the expected shot weight appear on the same drawing as the cavity layout. If those three numbers are on different documents, nobody owns the interface between machine and tool.

Reading a published shot range without being misled

Published machine data, including the ratings our own units carry, describes a capability envelope measured under stated conditions. It does not guarantee a process on your mold. The useful habit is to separate what each record proves from what a buyer typically assumes it proves.

Published recordConditions behind itWhat it can supportWhat it cannot support
Pour rate 20 to 500 g/s on a 1A1B seal unitPump and mixing head exercised across the band with a reference fluid at controlled temperatureScreening whether your shot weight falls inside the controllable bandThat a 13 g shot repeats within tolerance at the bottom edge
Metering accuracy ±0.3 percent, full rangeDynamic test across the full scaleComparing repeatability between machines at high outputAn accuracy claim at a small fraction of full scale, where valve response dominates
Component B control 90 to 115 °C for MOCA, 25 to 50 °C for BDOTank and line heating capabilityWhether your chain extender can be kept pumpable through a shiftYour cure schedule, which mold temperature and formulation decide
Vacuum to −0.095 MPa on the filled tankDegassing of material before it reaches the headWhether the component can be deaerated before meteringThat a 2 mm section will be void free, since air can enter at the gate
Ratio window about 100:8 to 100:13 for MOCAThe machine’s admissible ratio rangeWhether your formulation sits inside the machine’s capabilityThat ratio holds at the low end of the window through a long production run

The last row is the one that decides most projects. A machine that can be set to your ratio is not the same as a machine that holds it for six hours while tank temperatures drift and the pump wears. That difference only shows up in a run at production cycle, on your material, with the shot size you intend to use.

Proving the machine on your own seals

A trial is a measurement plan, not a demonstration. Decide what each check is meant to establish before the mold goes into the press, and write down the sample size, the test method and the person who signs the result. Otherwise the trial produces opinions about how the parts look.

What the first article should establish

  1. Shot weight repeat: weigh twenty consecutive shots at production cycle and record the spread, not the average alone.
  2. Hardness across cavities: test every cavity on the same scale, with specimens conditioned the same way, and report the range rather than a single part.
  3. Internal quality: section parts at the gate, at the last point to fill and at the thickest section, and inspect for voids and cold laps.
  4. Dimensions: measure the features that seal, on parts taken from the first, middle and last shots of the run.
  5. Demold: confirm parts release at the quoted cycle without tearing the lip or leaving ejector marks on a sealing face.
  6. Post-cure and end properties: after the specified post-cure, run compression set and oil resistance checks by the method agreed with your customer.

What a single-mold trial does not prove

One mold, one formulation and one shift prove that combination. A second tool with a different cavity count or runner volume shifts the shot, and a different colour paste or additive changes viscosity enough to move fill behaviour. A one-hour run also says nothing about thermal drift over a shift or pump wear over a season, which is where ratio errors usually begin. If a second product family is planned, trial it on the same machine before the order is placed, even if it means borrowing a sample mold.

The pour is only the first half of the cycle, and demold plus post-cure decide the properties the seal finally carries. <How Polyurethane Rollers Are Made From Casting To Cure> covers the casting to cure sequence on comparable 1A1B equipment.

The specification sheet to send before quoting

A quotation is only as good as the data behind it. Six fields carry most of the decision, and every one of them is something you can obtain before you approach a supplier.

RFQ fieldWhat to stateWhy it matters
Seal type and size rangeLip seal, rod seal, wiper or custom profile, with drawing and toleranceSets cavity volume and the flow path the material must travel
Cavity, runner and overflow volumeFrom the mold drawing, in cm³, with cavity countConverts to shot weight; without it the quote is a guess
Cured density and hardness targetSupplier cured density plus target hardness with test method and scaleDensity sets shot weight, hardness sets the ratio window and post-cure
Mix ratio and chain extenderPrepolymer, MOCA or BDO, ratio and permitted toleranceDetermines tank B temperature control, heat-up time and cleaning procedure
Cycle and demold requirementShots per hour, intended mold temperature, required demold timeDecides whether one head and one station are enough
Acceptance test listWhich checks, how many samples, who performs and signs themPrevents a trial that generates numbers nobody agreed to use

Reject this RFQ line: “1A1B PU casting machine, 500 g/s, suitable for polyurethane seals.”

Replace it with: prepolymer and chain extender identified; mix ratio with tolerance; shot weight per mold, cavity count and runner volume; the pour rate band the machine holds ratio within at that shot size; the metering accuracy basis; component B temperature range and heat-up time; vacuum level and degassing time; mold temperature interface; and the acceptance test list with sample size.

Check your seal shot before the machine is ordered

Send the seal drawing or size range, the cavity volume and cavity count, the runner and overflow volume from the mold drawing, the cured density, the target hardness with its test method, the mix ratio and chain extender, the shot weight per mold, the cycle you need and the mold temperature you intend to run. We will check that shot against the machine’s controllable band and check the tooling interface against the same numbers, before anyone calls a machine suitable.

Haifeng Polyurethane Machinery
Info@chinahaifeng.com
WhatsApp: 86 13566296633

FAQ

How do I size the shot range for small seals

Work from the material per mold, then compare it with the band the machine can control, not with its maximum. Calculate cavity volume times cured density times cavity count, add the runner allowance, and check where that number sits inside the published range. If your production shot falls in the lowest fifth of the range, ask for repeatability evidence at that size. A machine rated far above your shot will run, but the useful accuracy and the fill control you paid for may not be available where you need them.

Can one machine run both MOCA and BDO formulas

Usually yes, with conditions. Both routes need separate temperature bands, since MOCA must stay molten while BDO stays far cooler, and changeover means a full heat and purge cycle rather than a quick flush. Confirm the machine’s ratio window covers both formulations, that tank and line heating can reach the MOCA band and settle there, and that cleaning access reaches the mixing head and the lines that carried hardener. If the two families run in the same week, the changeover time belongs in your capacity calculation.

Why do seals show voids even after vacuum degassing

Tank degassing removes air from the component before metering. It cannot remove air that enters later. Voids usually come from a gate that jets into the cavity, a vent placed somewhere other than the last point to fill, a pour fast enough to fold air into a thin section, or a mold temperature low enough to freeze the leading edge and trap the air behind it. Moisture in fillers and insufficient vacuum time on a cold, viscous component also contribute. Section a part and locate the void before changing settings.

Does a higher pour rate improve seal quality

Rarely on its own. The fill time has to sit inside a window set by section thickness and pot life: too slow and the material gels before the cavity is full, too fast and it jets, entrains air or climbs the cavity wall unevenly. Higher rates help on thin, long-flow parts and on large shots where the cycle is dominated by fill. On a 15 g shot the difference between 20 and 40 g/s is a fraction of a second, and mixing quality and ratio stability matter far more.

How do I verify metering accuracy at my shot size

Weigh shots, and weigh the two components separately, at the shot size and cycle you will actually run. Take at least twenty consecutive shots so you see the spread rather than a single good result, and record tank and line temperatures alongside the weights so a drift can be traced. A ±0.3 percent figure quoted across the full range does not transfer to a small shot, because at that size the error budget is set by valve response and by how long the machine stays in steady flow.

If you’re interested, check out these related articles:

What Is Spray Polyurethane Foam Composition And Application
Causes Of Shrinkage In Polyurethane Foam How To Control It
SRIM Explained Structural Reaction Injection Molding Basics
RRIM Vs RIM Which Process Suits Your Structural Part
Measuring Polyurethane Foam Resilience A Practical Test Guide

Discuss Your Polyurethane Production Requirements

Share your application, material system, target output and automation requirements. Haifeng's engineering team can help you review equipment and production-line options. Our team will reply within one business day. Once requirements are clear, we provide a preliminary proposal within two business days.

Haifeng Polyurethane Machinery on TikTok
Haifeng Polyurethane Machinery on Instagram
Haifeng Polyurethane Machinery on Facebook
Haifeng Polyurethane Machinery on X
Haifeng Polyurethane Machinery on LinkedIn
Contact Haifeng Polyurethane Machinery on WhatsApp
Haifeng Polyurethane Machinery on YouTube